<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — Bed center problem]]></title>
		<link>https://www.soliforum.com/topic/11274/bed-center-problem/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/11274/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in Bed center problem.]]></description>
		<lastBuildDate>Mon, 25 May 2015 02:33:08 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: Bed center problem]]></title>
			<link>https://www.soliforum.com/post/96922/#p96922</link>
			<description><![CDATA[<div class="quotebox"><cite>rcskpeters wrote:</cite><blockquote><p>How am I able to change the pivot point? I have tried in Meshmixer and 123Desgin, but no luck. Do I need to use a different program? Or can I change the z-offset in slic3r for this model to something like -100?</p><p>Thanks!</p></blockquote></div><p>The z offset controls the height that the extruder starts at. If you want to center the model you would need to change the x and or y offset in slicer.</p>]]></description>
			<author><![CDATA[null@example.com (carl_m1968)]]></author>
			<pubDate>Mon, 25 May 2015 02:33:08 +0000</pubDate>
			<guid>https://www.soliforum.com/post/96922/#p96922</guid>
		</item>
		<item>
			<title><![CDATA[Re: Bed center problem]]></title>
			<link>https://www.soliforum.com/post/96920/#p96920</link>
			<description><![CDATA[<p>How am I able to change the pivot point? I have tried in Meshmixer and 123Desgin, but no luck. Do I need to use a different program? Or can I change the z-offset in slic3r for this model to something like -100?</p><p>Thanks!</p>]]></description>
			<author><![CDATA[null@example.com (rcskpeters)]]></author>
			<pubDate>Mon, 25 May 2015 02:29:14 +0000</pubDate>
			<guid>https://www.soliforum.com/post/96920/#p96920</guid>
		</item>
		<item>
			<title><![CDATA[Re: Bed center problem]]></title>
			<link>https://www.soliforum.com/post/96910/#p96910</link>
			<description><![CDATA[<p>The pivot point of the model is not in the center of the model. You can fix this in a modeling program.</p>]]></description>
			<author><![CDATA[null@example.com (barry1685)]]></author>
			<pubDate>Sun, 24 May 2015 22:02:55 +0000</pubDate>
			<guid>https://www.soliforum.com/post/96910/#p96910</guid>
		</item>
		<item>
			<title><![CDATA[Bed center problem]]></title>
			<link>https://www.soliforum.com/post/96907/#p96907</link>
			<description><![CDATA[<p>I need some help on a bed center problem with a model. I am trying to print a model from Thingiverse and it will not recognize the center of the bed. It keeps trying to print off the front left corner. I have tried using Netfab to fix it and Meshmixer as neither of them help. I have tried printing this using the XTZ software and also using Slic3r using settings that work with other models. </p><p>I am not familiar with gcode so I am not sure where to start with trying to figure out what the problem is. Any advice from others on how to fix this? The model is: <a href="https://www.thingiverse.com/thing:758630/#instructions">https://www.thingiverse.com/thing:758630/#instructions</a></p><p>Thanks!<br />Ryan</p>]]></description>
			<author><![CDATA[null@example.com (rcskpeters)]]></author>
			<pubDate>Sun, 24 May 2015 21:30:20 +0000</pubDate>
			<guid>https://www.soliforum.com/post/96907/#p96907</guid>
		</item>
	</channel>
</rss>