Topic: calibrating correct coordinates for virtual build table in simplify 3d
I am running rep .092 and I have the most difficulty printing large objects because I can't get them to align in the center of the bed. My live preview shows the object in the center of the bed but when I print the object is not aligned correctly and sometimes the extruder extrudes off the bed. I've tried gcode offsets but I think some objects its different based on the pivot point. Is there a setting I am missing somewhere in simplify 3d to set up bed corner coordinates?