Topic: Quick question about infill gaps.
Hey everyone I got my 3d printer recently and am pretty happy with the results, setting it up is a fairly easy process and I spent a good hour or 2 getting it calibrated and printing a few small test prints. I am happy with the quality at 0.2mm and 0.1mm layer height, however I have a concern and I was just wondering if you guys had any input on this. OK so basically In the images I attached it is visible that there are small gaps around the holes in my prints also you can kind of see through the top layer and see the little mesh pattern from the layer below. Is this the slicer or the firmware? Or is it something I need to physically adjust on the printer. I am really happy with the prints it makes I just feel as though this is an issue that should be pretty easy to fix. Thanks and any input is appreciated.
p.s. I have a davinci 1.0 with 1.2.7 firmware and the latest windows program.