Topic: Solidoodle 2 thermistor problems (extruder AND bed)
Hello,
First, my setup:
- Solidoodle 2
- Sanguinololu with 644p
- Pico hot-end
- RepetierHost
A couple weeks ago, I had a long-running print go awry. I made the stupid mistake of using solid-core wire for the hot-end cooling fan, and it developed a break about 20% into a 9 hour print.
I also made the mistake of not keeping an eye on the print. I woke up the next morning to find that the filament (PETG) had jammed and the extruder stepper continued to feed the filament, but not into the hot-end, but out the front, leaving me with a nice big ball of unusable filament.
I unplugged the printer and switched over to using my other printer for the project.
Today, I decided to plug the Solidoodle2 back in and found a few things really disconcerting.
1) Repetier is currently telling me that the hot-end is at 88C (though it is at room temperature)
2) Repetier is also telling me that the print bed is at 91.3C (it too is at room temperature)
3) I daringly ran through the auto-pid tuning routine, and while the hot-end was at (supposedly) 200C, I was able to manually push through a bunch of PETG which came out very very "liquidy" (I'm guessing it was a LOT hotter than 200C)
I've measured the bed thermistor and it reads somewhere around 70-80k ohms, and the same for the hot-end thermistor.
Does anyone have any ideas/suggestions?
Thanks in advance