Topic: Stumped. Rep .092 and S3D Medium speeds and print failing at infill
So I am running a Davinci 1.0a MK9 extruder with .092 REP and slicing via S3D. On slow speeds I can print small objects with infill of 30% fine. But I am stuck problem solving a larger print with medium speeds. The extruder works for the first 3-4 layers until it reaches the infill, once it hits this point the infill looks choppy and my extruder is in the air not extruding any filament.
If I push down on the filament the extruder will start extruding once again in the air, so this tells me something is going on at the infill section and causing the filament to stop pushing through the feeder. I am totally stumped..