Topic: Solidoodle 4 pauses printing; resumes almost immediately
Hi guys! I purchased a Solidoodle 4 last year and it's been working great the whole time.
Just recently, I've been printing pulley sleeves and it's been randomly stopping during prints. There is still plastic oozing out of the nozzle when it stops, but the extruder itself doesn't move, leaving a very small but inconvenient blob on the surface. Not even a second later, it resumes printing.
What would be the main cause of this as it has never happened before? I suspect it might be software issue and not a hardware issue.
During the print, I was printing black ABS on hairspray/kapton tape (210 deg C @ nozzle; 110 deg C @ heatbed)