Okay so uses what temperatures for small medium prints in different materials?
Just run off a print and only realized near the end it was at 260 on the extruder and 95 on the bed and gave a really good finish
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → XYZ Printing DaVinci → Printing Temp
Okay so uses what temperatures for small medium prints in different materials?
Just run off a print and only realized near the end it was at 260 on the extruder and 95 on the bed and gave a really good finish
I've been using various filaments lately such as Woodfill, Bronzefill and PLA.
I find the bed is fine at 60°C for everything provided it's levelled correctly and using the glue stick.
For the extruder, I use 215 for Woodfill and 220 for PLA and Bronzefill.