I left a print running while i went to watch a local hockey game.  It looks like if started to fail about an hour into a three hour print.  I can't tell what happened yet. I hope nothing broke.

Post's attachments

IMG_20150314_223904.jpg
IMG_20150314_223904.jpg 2.43 mb, file has never been downloaded. 

IMG_20150314_223909.jpg 2.33 mb, file has never been downloaded. 

IMG_20150314_223916.jpg
IMG_20150314_223916.jpg 2.69 mb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

2

Re: Epic fail

No sufficient adhesion, I think

Fat kids are harder to kidnap!

3

Re: Epic fail

Yep, that's what I get when the part comes unstuck from the print bed and shifts. Suddenly it is printing in air instead of on previous layers :-).