Topic: Epic fail
I left a print running while i went to watch a local hockey game. It looks like if started to fail about an hour into a three hour print. I can't tell what happened yet. I hope nothing broke.
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → Solidoodle Press → Epic fail
I left a print running while i went to watch a local hockey game. It looks like if started to fail about an hour into a three hour print. I can't tell what happened yet. I hope nothing broke.
No sufficient adhesion, I think
Yep, that's what I get when the part comes unstuck from the print bed and shifts. Suddenly it is printing in air instead of on previous layers :-).