Topic: Layer issue
Right guys used the Hobbyking Esun filament to print this using the following settings:
Layer Height - 0.3
Density - 10%
Speed - Normal
But some areas seem to of 'split' I have attached the images of it to show what I mean...
Any help would be grateful thank you