1 (edited by efes 2015-06-22 20:14:04)

Topic: davinci 1.0 warm cabin ?

hello,

I believe that because of the heat in the cabin engines do not!
when it's too hot it does not work very well for doing his continuous stops quickly?
people who use a fan to clear heat from the cabin? if so how?
thank you

sorry english not good ! use translate hmm

add setup simplify3d please look normal config or not normal ?

during this test door open with open top too!

probleme video : https://youtu.be/BbS5hlbCKr0


[video]





cube test no problem ?

https://youtu.be/X4uwg7xZpx8
speed 220 !


I understand anything ?

Post's attachments

20150622_220240 [800x600].jpg
20150622_220240 [800x600].jpg 30.59 kb, file has never been downloaded. 

singlewalllcylindersimplify3dsetup.fff 9.36 kb, 3 downloads since 2015-06-22 

You don't have the permssions to download the attachments of this post.
davinci 1.0
firmware repetier

2

Re: davinci 1.0 warm cabin ?

for good ....
I printed a 20cm long cylinder with ONLY 3 small mini stop not too serious!
I believe that my first file was not good!
http://soliforum.com/i/?ff7GOX8.jpg

davinci 1.0
firmware repetier

3

Re: davinci 1.0 warm cabin ?

efes,

The problem you have could be due to a slow computer.  If your computer is running other things while your printing, it could cause the software to slow down too, which then makes the printer skip and mess up.
I would suggest, before you start a print, to restart your whole computer and not open anything up except for Simplify3D, and see if that makes a difference.

Hope this helps,
Dom

Da Vinci 2.0 with Repetier Firmware (Printing in ABS/PLA/Exotics)
12 Years PC Experience
16 years old