<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — davinci 1.0 warm cabin ?]]></title>
		<link>https://www.soliforum.com/topic/11567/davinci-10-warm-cabin/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/11567/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in davinci 1.0 warm cabin ?.]]></description>
		<lastBuildDate>Tue, 23 Jun 2015 00:15:50 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: davinci 1.0 warm cabin ?]]></title>
			<link>https://www.soliforum.com/post/99678/#p99678</link>
			<description><![CDATA[<p>efes,</p><p>The problem you have could be due to a slow computer.&nbsp; If your computer is running other things while your printing, it could cause the software to slow down too, which then makes the printer skip and mess up.<br />I would suggest, before you start a print, to restart your whole computer and not open anything up except for Simplify3D, and see if that makes a difference.</p><p>Hope this helps,<br />Dom</p>]]></description>
			<author><![CDATA[null@example.com (Dominick)]]></author>
			<pubDate>Tue, 23 Jun 2015 00:15:50 +0000</pubDate>
			<guid>https://www.soliforum.com/post/99678/#p99678</guid>
		</item>
		<item>
			<title><![CDATA[Re: davinci 1.0 warm cabin ?]]></title>
			<link>https://www.soliforum.com/post/99640/#p99640</link>
			<description><![CDATA[<p>for good ....<br />I printed a 20cm long cylinder with ONLY 3 small mini stop not too serious!<br />I believe that my first file was not good!<br /><span class="postimg"><img src="http://soliforum.com/i/?ff7GOX8.jpg" alt="http://soliforum.com/i/?ff7GOX8.jpg" /></span></p>]]></description>
			<author><![CDATA[null@example.com (efes)]]></author>
			<pubDate>Mon, 22 Jun 2015 20:48:01 +0000</pubDate>
			<guid>https://www.soliforum.com/post/99640/#p99640</guid>
		</item>
		<item>
			<title><![CDATA[davinci 1.0 warm cabin ?]]></title>
			<link>https://www.soliforum.com/post/99625/#p99625</link>
			<description><![CDATA[<p>hello,</p><p>I believe that because of the heat in the cabin engines do not!<br />when it&#039;s too hot it does not work very well for doing his continuous stops quickly?<br />people who use a fan to clear heat from the cabin? if so how?<br />thank you</p><p>sorry english not good ! use translate <img src="https://www.soliforum.com/img/smilies/hmm.png" width="15" height="15" alt="hmm" /></p><p>add setup simplify3d please look normal config or not normal ?</p><p>during this test door open with open top too!</p><p>probleme video : <a href="https://youtu.be/BbS5hlbCKr0">https://youtu.be/BbS5hlbCKr0</a></p><br /><p><a href="BbS5hlbCKr0">[video]</a></p><br /><br /><br /><br /><p>cube test no problem ?</p><p><a href="https://youtu.be/X4uwg7xZpx8">https://youtu.be/X4uwg7xZpx8</a><br />speed 220 !</p><br /><p>I understand anything ?</p>]]></description>
			<author><![CDATA[null@example.com (efes)]]></author>
			<pubDate>Mon, 22 Jun 2015 17:41:29 +0000</pubDate>