Topic: can't make ABS slurry
Nothing seems to be working for me when it comes to 3d printing.
I got few failed prints printed by my Solidoodle 4 with the ABS Solidoodle filament with no colorants, put it in a jar and poured some clear acetone in there, as everyone says.
Two days later, this:
it's like soft parts of bread in water. The are extremely soft and squishy but don't dissolve and form a creamy substance no matter how much I shake and mix them.