1

Topic: Xyz keeps restarting help please

Ok, so i had a print a few nights ago and my printer was on for a while. The print was finished and looked great! Now my davinci 1.0 will work, but it restarted at random items within around 5 to 20 seconds.... I tried to reinstall the firmware and nothing.  I cut the cables to the extruder off and took off my fan, still does the same thing.. I was thinking maybe the PSU is going bad? Any ideas?

https://www.youtube.com/watch?v=leRMsyKRWzU

not the best quality

2

Re: Xyz keeps restarting help please

Well, looking at the video, it seems like your thermistors is showing 1 degree at room temperature. If you are not keeping it in the fridge, it should show the ambient temperature before you start heating it up. So it might be a brake or short in the thermistor. Did you by chance cleaned your hotend with the wire brush? - It might have shorted it if some damage occurred to the thermistor connection. Anyway, just a guess based on limited information. I think I read somewhere that Da vinci will continue restarting if something wrong with the thermistor.

3

Re: Xyz keeps restarting help please

it was 1 degree because it was unhooked. I put a new PSU and new hot end on just now and get the same thing

4

Re: Xyz keeps restarting help please

https://www.youtube.com/watch?v=zRUlW6LaCik

with the new nozzle and psu =P

I just don't get why it would mess up like that

5

Re: Xyz keeps restarting help please

Does this happen on sample files or just files you create?

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

6

Re: Xyz keeps restarting help please

it happens if it is just idle

7 (edited by Vxxs 2015-06-11 18:18:25)

Re: Xyz keeps restarting help please

i was just warming up the extruder

8

Re: Xyz keeps restarting help please

Well that leaves either a bad power supply or you have a short in the 12 volts section of the heater circuit. My guess is the later. Make sure the wires on the heater are not exposed and touching each other or touching the brass heat block. But if it happens when just idle that points back the the supply.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

9

Re: Xyz keeps restarting help please

I wired up my old atx psu, it does seem to restart more often when you heat up the extruder.  I put the extruder on top of the printer and still get the reset...  It's almost the same as when you clean with a wire brush and it resets. I tried to see if i had a bad wire or any connection on the heat block... Maybe my motherboard is bad?

10

Re: Xyz keeps restarting help please

Vxxs wrote:

I wired up my old atx psu, it does seem to restart more often when you heat up the extruder.  I put the extruder on top of the printer and still get the reset...  It's almost the same as when you clean with a wire brush and it resets. I tried to see if i had a bad wire or any connection on the heat block... Maybe my motherboard is bad?

You know you are only supposed to use the wire brush when power is not applied to the extruder. Such as right when a print finishes and it is still hot but unpowered. Several users here have blown out there controllers because there are live exposed wires right at the base of the heater. Short those with the brush and you put a short across the boards 12 volt rail.

Too late to tell you this know however..

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

11

Re: Xyz keeps restarting help please

I did rest it in the past with the wire brush, but that was months ago.  This last print was 12 hours and successful, it was just restarting when i came home.  So you think maybe someyhing blew out the controller? So its scrap then

12

Re: Xyz keeps restarting help please

I just dont get why it can heat up to around 100c

13 (edited by carl_m1968 2015-06-12 00:23:50)

Re: Xyz keeps restarting help please

Vxxs wrote:

I did rest it in the past with the wire brush, but that was months ago.  This last print was 12 hours and successful, it was just restarting when i came home.  So you think maybe someyhing blew out the controller? So its scrap then


Not necessarily. Most of the ones that blew out where repairable depending on the version of your controller. Where the 12 volts plugs in at which is a white connector with yellow and black wires, there are a couple of surface mounted resistors. Those should measure near short as they are zero ohms and being used as fuses. If one or more of those measure high as in several hundred ohms or more then they have burned as they should. Depending on your soldering skills you can order replacements from mouser or digikey and replace them. If those are not blown then the issue lies deeper in your board in which case yes the board is scrap.

One last thing you could do is measure the resistance across the heater. Unplug it at the top of the extruder and use a meter to measure from pin to pin in that connector. Its a 40 watt heater running at 12 volts so the resistance should be right around 3.33 ohms. If it is lower that is bad.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.