Topic: Offbrand Filament problems for Solidoodle Press
I ran out of Solidoodle filament. I tried using my local computer shop's filament (Microcenter brand), however I'm having trouble. The filament extrudes fine while the print head is at the home state and I'm using the Soliprint Extrude 50mm command. However when I begin printing, the filament jams and stops producing.
I'm not sure what causes this. Is it bad filament? is there a temperature drop when I begin my print? Has anyone else had this problem?
I'm using Microcenter ABS Filament,
Printing at 240-255 degrees, Extrudes perfectly when doing a 50mm extrude. Printing jams.
Bed temp 90-105
thanks