Topic: Need advice before attempting to print with Taulman Bridge.
Hi, I'am running Da Vinci 1.0 with Rep firmware and e3d mod. I have been successfully printing with ABS, PLA-PHA, Woodfill, XT. I'am about to try Taulman Bridge. Someone with a similar setup - what temperature extruder/bed should I use? Also, my print-bed is covered with Kapton, I rather not remove it, should I just apply some dilute PVA, let it dry and then print? Any advice is welcomed.