Topic: PLA Success with Press
Thought I would try out some PLA, because the Press is supposed to be able to print it, right?
So I knew I was up against it with having no part fan, my printer is bone stock with no modifications (yet) and I as said before no part fan. See pictures below, I'm fairly happy with the results and the results are repeatable and the print quality seems repeatable.
3d Filaprint (Rep-Rapper) Gold PLA (1.75)
0.2 Layer Height
95 bed
200 extruder
top open
door open about 3"
Hope this helps people that are having difficulties with PLA, this has been successful for me.
Rob