1

Topic: Was FW version E the one that did not track the filament? On the 1.0.

I have the da vinci 1.0 and I am wanting to drop back on FW so I don't need the resetter. Was E the one that did not keep track if the filament?

Thanks.

2

Re: Was FW version E the one that did not track the filament? On the 1.0.

Why not flash to Repetier 9.2? You dont even need to unscrew the back of the printer to get to the motherboard to flash it. Repetier is also way better than the stock firmware

3

Re: Was FW version E the one that did not track the filament? On the 1.0.

ArcticWolf_11 wrote:

Why not flash to Repetier 9.2? You dont even need to unscrew the back of the printer to get to the motherboard to flash it. Repetier is also way better than the stock firmware

I have thought about that also but I use S3d and thought there was a problem with Repetier and S3D on the Da Vinci.

4

Re: Was FW version E the one that did not track the filament? On the 1.0.

rforeman wrote:
ArcticWolf_11 wrote:

Why not flash to Repetier 9.2? You dont even need to unscrew the back of the printer to get to the motherboard to flash it. Repetier is also way better than the stock firmware

I have thought about that also but I use S3d and thought there was a problem with Repetier and S3D on the Da Vinci.


S3D works with virtually any printer and any firmware. There is a reason it sets you back 150 bucks.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

5

Re: Was FW version E the one that did not track the filament? On the 1.0.

I'm using E and can confirm it doesn't count filament.

Davinci 1.0 with repetier firmware & E3D V6 Lite
Anycubic Photon DLP printer, Einscan-S 3D scanner
Simplify3d, 123D Design, Meshmixer
http://www.thingiverse.com/scobo/designs

6

Re: Was FW version E the one that did not track the filament? On the 1.0.

Just remember that XYZ considers it a warranty violation to not upgrade to the most recent version. Thats why they ask you what your current version is when making a warranty claim. Dumb if you ask me but that is their business model..

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

7

Re: Was FW version E the one that did not track the filament? On the 1.0.

Why does that not surprise me. roll

Davinci 1.0 with repetier firmware & E3D V6 Lite
Anycubic Photon DLP printer, Einscan-S 3D scanner
Simplify3d, 123D Design, Meshmixer
http://www.thingiverse.com/scobo/designs

8 (edited by rforeman 2015-05-23 16:44:51)

Re: Was FW version E the one that did not track the filament? On the 1.0.

Thanks Guys. I dropped it back to Version E for the time being. At some point I am going to do a major mod on it. I may try Repetier 9.2 soon. Last night the glass chipped, so now I have to replace the heat bed. Of course XYZ is out of stock on the bed so I need to figure out what I am going to do to fix it. I got this printer back in August last year but have long sense gave XYZ the I think they are #1 sign as far as their warranty goes.

carl,
Are you still going to do w write up on the conversion you did on yours. I would like to do the same thing you did but, I am still very new to this and having a hard time trying to figure out where to start as far as modding goes.

9 (edited by carl_m1968 2015-05-23 17:10:00)

Re: Was FW version E the one that did not track the filament? On the 1.0.

rforeman wrote:

Thanks Guys. I dropped it back to Version E for the time being. At some point I am going to do a major mod on it. I may try Repetier 9.2 soon. Last night the glass chipped, so now I have to replace the heat bed. Of course XYZ is out of stock on the bed so I need to figure out what I am going to do to fix it. I got this printer back in August last year but have long sense gave XYZ the I think they are #1 sign as far as their warranty goes.

carl,
Are you still going to do w write up on the conversion you did on yours. I would like to do the same thing you did but, I am still very new to this and having a hard time trying to figure out where to start as far as modding goes.

Getting close, still having a few minor bugs pop up in some prints. Once i get rid of those and can print reliably I will make a write up.

My bed chipped as well. All I did is got a local glass company to cut and edge polish to pieces of tempered glass that where the same size as the stock piece but 3mm thick. I simply mounted one on top of the existing piece and added 3mm to my z offset. No issues since.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

10

Re: Was FW version E the one that did not track the filament? On the 1.0.

carl_m1968 wrote:
rforeman wrote:

Thanks Guys. I dropped it back to Version E for the time being. At some point I am going to do a major mod on it. I may try Repetier 9.2 soon. Last night the glass chipped, so now I have to replace the heat bed. Of course XYZ is out of stock on the bed so I need to figure out what I am going to do to fix it. I got this printer back in August last year but have long sense gave XYZ the I think they are #1 sign as far as their warranty goes.

carl,
Are you still going to do w write up on the conversion you did on yours. I would like to do the same thing you did but, I am still very new to this and having a hard time trying to figure out where to start as far as modding goes.

Getting close, still having a few minor bugs pop up in some prints. Once i get rid of those and can print reliably I will make a write up.

My bed chipped as well. All I did is got a local glass company to cut and edge polish to pieces of tempered glass that where the same size as the stock piece but 3mm thick. I simply mounted one on top of the existing piece and added 3mm to my z offset. No issues since.