L.woinson95 wrote:Have you got the correct settings at hand or not? Or would I have to mess around with it
There is no correct setting. What you have to do is measure like 50mm of filament at the extruder input. Then command it to feed 50mm and see how close it is. If it falls short then add steps. If it is too much then remove steps.
The issue is there are variations in motors, the amount of pressure the idler applies and the softness of filament that affect the setting.