1

Topic: What Is The Best Extruder And Bed Temperature For ABS?

Well can you just tell me what temperature you have your Da Vinci set to. Thanks

2

Re: What Is The Best Extruder And Bed Temperature For ABS?

Need to specify what ABS you are using (manufacturer, color, etc).  The optimal setting for my spools vary from 195C to 240C.

3

Re: What Is The Best Extruder And Bed Temperature For ABS?

right now im using the standard filament that the Da Vinci came with and after thats done I will use Hatchbox white filament

4

Re: What Is The Best Extruder And Bed Temperature For ABS?

I would really advise against using white in any brand. I have never been able to get white to print well regardless of brand. The pigment that is used just makes the temperature and speed requirements very hard to dial in.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

5

Re: What Is The Best Extruder And Bed Temperature For ABS?

really?, because when I print out in white it turns out pretty decently to me, the color is more of a cream white when printed for me, unless that isn't what is supposed to be. But im' using white so I can paint it easily

6

Re: What Is The Best Extruder And Bed Temperature For ABS?

ArcticWolf_11 wrote:

really?, because when I print out in white it turns out pretty decently to me, the color is more of a cream white when printed for me, unless that isn't what is supposed to be. But im' using white so I can paint it easily


Try printing with natural if you think white looks good. Natural should blow you away. It to can be painted. Oh and white should come out white. if it is coming out darker then you are cooking it with too much heat. The stock stuff that you get in cartridges should not be printed at higher than 190. It is not the typical formulation and they had it specially made to print at lower temps than normal.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

7

Re: What Is The Best Extruder And Bed Temperature For ABS?

oh okay so what do you recommend that I print at using the Hatchbox filament?

8 (edited by kszwab 2015-05-12 21:31:10)

Re: What Is The Best Extruder And Bed Temperature For ABS?

220-230C extruder, 90C bed Davinci 1.0

220-230C extruder, 70C bed Davinci Duo

9

Re: What Is The Best Extruder And Bed Temperature For ABS?

I've been running 210 and 90. Fine for me.

10

Re: What Is The Best Extruder And Bed Temperature For ABS?

I have been printed esun stuff at 215 and I think it is ok, what are the signs saying it is not hot enough?
I agree my white never looks as good as my colours printed at same temps

11

Re: What Is The Best Extruder And Bed Temperature For ABS?

I am still tweaking my settings, but I am printing ABS white, can't remember from where at the moment.
Extruder is at 230, bed at 130

RoVa3D with five nozzles (first nozzle down, four to go)
Slic3r and Pronterface
Filastruder and Filawinder - soon enough
Current hurdles - humidity, offsets

12

Re: What Is The Best Extruder And Bed Temperature For ABS?

MyMultiExtruder wrote:

I am still tweaking my settings, but I am printing ABS white, can't remember from where at the moment.
Extruder is at 230, bed at 130

From what I see of your signature you are not using  Da Vinci. The Da Vinci bed cant get to that temp and if it did the plastic frame would be damaged.   Honestly I have never heard of a bed temp of more than 110 for any material.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

13

Re: What Is The Best Extruder And Bed Temperature For ABS?

carl_m1968 wrote:
MyMultiExtruder wrote:

I am still tweaking my settings, but I am printing ABS white, can't remember from where at the moment.
Extruder is at 230, bed at 130

From what I see of your signature you are not using  Da Vinci. The Da Vinci bed cant get to that temp and if it did the plastic frame would be damaged.   Honestly I have never heard of a bed temp of more than 110 for any material.

Yes, true. I'm not using Davinci. Your title wasn't specific to Davinci, and I didn't notice you had specified a brand in your post until now. I wasn't meaning to derail the topic smile still getting used to the forums, and I see that there is a forum specific for printer brands. Sorry smile

RoVa3D with five nozzles (first nozzle down, four to go)
Slic3r and Pronterface
Filastruder and Filawinder - soon enough
Current hurdles - humidity, offsets

14

Re: What Is The Best Extruder And Bed Temperature For ABS?

MyMultiExtruder wrote:
carl_m1968 wrote:
MyMultiExtruder wrote:

I am still tweaking my settings, but I am printing ABS white, can't remember from where at the moment.
Extruder is at 230, bed at 130

From what I see of your signature you are not using  Da Vinci. The Da Vinci bed cant get to that temp and if it did the plastic frame would be damaged.   Honestly I have never heard of a bed temp of more than 110 for any material.

Yes, true. I'm not using Davinci. Your title wasn't specific to Davinci, and I didn't notice you had specified a brand in your post until now. I wasn't meaning to derail the topic smile still getting used to the forums, and I see that there is a forum specific for printer brands. Sorry smile

I figured as much, no biggie. Just was saying as a general statement that Da Vinci could not reach that temp to avoid confusion. I thoughy maybe you had a Da Vinci and was just ashamed to admit it.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.