Topic: PLA Sticks - ABS Not
Been using mostly PLA for near 18 mo. Got it to where I need a razor blade and a little assistance to get the print off the heated - Aqua Netted glass. Just got 2 new rolls of ABS to hopefully create Lawsys' carriages. I can't get the whole print to stick for love nor money. Printing at 210/95, then 210/90 - /85 - /80 pretty much the same - won't entirely stick down. Have messed with Z height, even set all of the VREF settings. Now I have nice smooth sided prints, but one or more corners won't stick and warps, or the print just eventually comes loose. Got a little bit better with some blue printers tape, still won't fully stick.
Suggestions??
TIA
Ski
PS - for those that haven't yet checked the VREF settings - do so! My extruder alone was factory set to .85 - (same) factory recommends .25 - made a noticible difference. Got the others to 1.03, 1.04, etc need to be 1.0 - hafta do a little more. Need better light AND a plastic screwdriver...... Maybe I'll print one........??