Topic: Extruder issues - Clicking???
I have three daVinci printers. One has begun to give me a some problems lately and I cannot figure it out. It will begin a print, build about 1/4" high, then start clicking and no filament being extruded.
I use Sainsmart 3rd party filament with no issues in the other machines.
I calibrated the bed and tried using the stock XYZ filament to build the sample star vase and STILL would only build 1/4" high before failure.
I then tried the 3rd party filament at a higher temp (230) and got the same failure results.
What am I doing wrong, or are there any solution to fix this problem?
Many thanks,