Topic: Later shift, maybe?
So I've run into a problem that arises where every 4 layers or so the outer shell layer sticks out a bit. However this only happen for layers between 30-150 and then stops and prints no problem. I did a full re-tentioning of the belts and the problem still persists, but the other thing is that it only occurs on certain models, I've printed models 8" high with no problem and yet some models have layer shift between layers 30-150. See image below.