Topic: Extruder temperature limited to 230 degrees C in Davinci 1.0A
Esun filament operates from 220 to 260 degrees C according to the box.
The esun filament is wound into the original XYZ printing cartridge.
By reprogramming the cartridge eeprom I tried increasing the temperature of the extruder to 245, then 240 then 235.
None of these temperature settings worked - the extruder started at a high temperature with auto heat and gradually the extruder temperature went down to ambient.
The only temperature that worked was 230 degrees C, the readings on the XYZ ware panel showed 236 degrees C.
FW version is 1.0.1 and XYZ Ware is 1.1.32.1
Is the FW limiting the temperature to 230 degrees C?
Has anyone succeeded in getting higher than 230 degrees C with stock software?