1

Topic: Davinci Massive offset printing

So I have updated the Davinci 1.0a to the latest .92 repetier.  Was printing along great.  Lots of great printing.  Then one was shifted.  Thought nothing of it till it got progressively worse.  Now I cant print anything without the print head moves on the x axis but the y axis is still moving a bit.  I have uploaded firmware several times even reverting back to xyz firmware.  cant seem to get a goo xyz to work either.  Checked belt tensions, Stepper motor wiring swaps.  I am including a picture of the last print I tried.  first layer is where this goes all wrong every print no matter what slicer I am using.  HELLLPPP!!!!!! lol

Post's attachments

image1.JPG
image1.JPG 514.93 kb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

2

Re: Davinci Massive offset printing

3dchromeconcepts wrote:

So I have updated the Davinci 1.0a to the latest .92 repetier.  Was printing along great.  Lots of great printing.  Then one was shifted.  Thought nothing of it till it got progressively worse.  Now I cant print anything without the print head moves on the x axis but the y axis is still moving a bit.  I have uploaded firmware several times even reverting back to xyz firmware.  cant seem to get a goo xyz to work either.  Checked belt tensions, Stepper motor wiring swaps.  I am including a picture of the last print I tried.  first layer is where this goes all wrong every print no matter what slicer I am using.  HELLLPPP!!!!!! lol

Looks like you have some steppers that are dying if you have tried all of the above and it looks good after it is sliced.

3

Re: Davinci Massive offset printing

you think so even after it side steps it continues to print?...i've noticed that the x and y axis displayed on the screen are true to where it should be not where it actually is.

4

Re: Davinci Massive offset printing

I had issues with the slicer.  Are you printing with a file you have printed successfully before?

5

Re: Davinci Massive offset printing

super common issue with 1.0A on .92.... No solution yet...

http://voltivo.com/forum/davinci-peersu … port-group

6

Re: Davinci Massive offset printing

humanisticnick wrote:

super common issue with 1.0A on .92.... No solution yet...

http://voltivo.com/forum/davinci-peersu … port-group

I use .91 on my 1.0 and have never seen this issue.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

7

Re: Davinci Massive offset printing

The problem is narrowed down to 1.0A and RH .92.  It doesn't pertain to the 1.0's



carl_m1968 wrote:
humanisticnick wrote:

super common issue with 1.0A on .92.... No solution yet...

http://voltivo.com/forum/davinci-peersu … port-group

I use .91 on my 1.0 and have never seen this issue.