Topic: XYZerocart Update + results of testing
I purchased the XYZerocart for my davinci 1.0, in hopes of freeing me from the need of purchasing XYZ filament, however I also did not want to void my warranty either. I also did not want to downgrade my firmware from version 1.2.5.
I was successful.
I am happy to report the firmware 1.2.5 works perfectly with the xyzerocart. I have set settings back and forth, and the davinci reads them all with no issues. A few things of note however you might want to keep in mind. First, I do not use xyzware, I use Simplify3d to communicate with the printer. Therefore I have no worries about having xyz disable my printer as the Simplify software does not talk to XYZ at all. (Simplify3d is also a HUGE improvement and makes much better prints than the stock xyzware, its worth the investment)
I also found a great terminal program to communicate with the xyzerocart, its called quick terminal for android and runs right on my phone. Quick easy and fast to set the filament length every so often.
All in all, I have not modified my printer at all yet I am free of XYZ's attempts to force me into their expensive filament. Mission successful.....
-Steve