Topic: Cube Feedback
Hello All
Well, after changing the hairspray I used I was able to complete Z Calibration and immediately printed a cube to see what the score was, this is what I got ![]()
I was quite pleased with the result for a VERY first print, but would like some feedback from some pro's. I'm ware of the moire and I know what I need to do to get rid of it, however it seems my layers looking from the top are seperated, what causes this? and how do I fix it. Also there seems to be 'tiny' gaps between the indents of the moire, is this related?
I was quite pleased with the sizing, this is printed using soliprint v1.1.1 with 215 degree hot end and 93 degree bed at 300 micron using default everything else. The size was measured with calipers at 25mm square +/- 0.5mm. I was quite please with that or should I be expecting 25mm dead at 0.3?
Thanks for any help