Topic: Extruder pulse moire at 1/32 microstepping causing diagonal lines?
[solved] - see post #10 = http://www.soliforum.com/post/86633/#p86633
Hey guys, I could use a little help on this one because it's about to drive me mad trying to solve it. I get what appear to be very regular extruder pulses causing diagonal lines in my prints. I'm using a RUMBA at 1/32 microstepping on 8825's and originally got it to help solve this issue similar hoping to get something similar to Ian's results (http://www.soliforum.com/post/33357/#p33357) - but no such luck.
I would consider the rest of my printer pretty highly tuned and the regularity makes me think it's either a slicer issue (Slic3r 1.1.7) or something in the Gcode.
Pictures attached of 20x20x50 shells - how do I get rid of this?
*I suggest opening the images in a new tab for superior zoom



Thanks