Topic: Filament not sticking
Getting closer to my first print! My issue right now is the extruder. I started out with black set at 195 degrees C. The plastic came out of the nozzle and curled up around the tip. I read there was some problems with the black in the early days (and I do have early black) and that you should try a temp around 205. Didn't help.
I switched to white, reset to 200 degrees and had the same problem.
In both cases I thought it might have been that the plastic needed to be laid down, that it was normal to come out of the nozzle and curl. However the plastic didn't stick to the bed, all it did was curl up around the tip, so I shut it down before it built up too much.
I didn't see anything on this site about this problem but it did seem like part of the problem may be a partially clogged nozzle. Will get something to clean it out next time I go out. Does however seem to me that the plastic should have stuck to the bed so there might be another problem.
Any thoughts appreciated