Topic: Layer alignment issues with Avatar IV 3D Printer
I just bought my first 3D printer, an Avatar IV, from a Chinese manufacturer. I've been testing the printer for the past few days without enjoying much success in terms of layer alignment. There is an offset between each layer printed.
I'm trying to print the part shown on picture 3D Part.jpg.
The results are shown on the three other pictures.
I have been printing with PLA filaments. My printing settings are:
One Extruder
Extruder Temperature: 200°C
Hot Bed Temperature: 50°C (Glass covered by blue tape)
Object Infill: 10%
Layer Height: 0.27mm
Number of Shells: 1
Feedrate: 40mm/s
Travel Speed: 30mm/s
I would like to know what might cause this improper layer alignment and how I can fix it. Thank you!