26

Re: so been away awhile, first layer not sticking!!!!!!!

does yours have a prob that you reset on each print for the auto lvl ?

• Solidoodle Workbench Apprentice
• Creates plastic parts up to 6" x 6" x 8"
• Heated Aluminum Build Platform with Glass Bed
• Dual extruder

27

Re: so been away awhile, first layer not sticking!!!!!!!

cpsmicahel wrote:

does yours have a prob that you reset on each print for the auto lvl ?

Are you sure you're posting to the correct topic? 
He has an SD3 and is having some calibration issues.
Your posts would be helpful if he had a workbench such as yourself.

Printit Industries Model 8.10 fully enclosed CoreXY, Chamber heat
3-SD3's & a Workbench all fully enclosed, RH-Slic3r Win7pro, E3D V6, Volcano & Cyclops Hot End
SSR/500W AC Heated Glass Bed, Linear bearings on SS rods. Direct Drive Y-axis, BulldogXL
Thanks to all for your contributions

28

Re: so been away awhile, first layer not sticking!!!!!!!

i guess not then

• Solidoodle Workbench Apprentice
• Creates plastic parts up to 6" x 6" x 8"
• Heated Aluminum Build Platform with Glass Bed
• Dual extruder

29

Re: so been away awhile, first layer not sticking!!!!!!!

so I fixed my issues, lol I just switched to PLA instead. lol
ABS sux

30

Re: so been away awhile, first layer not sticking!!!!!!!

ABS is king you should get it working wink

31

Re: so been away awhile, first layer not sticking!!!!!!!

so its printing well with ABS, but the resolution of the layers is horrible. they are rough.
any ideas why this is happening.

32

Re: so been away awhile, first layer not sticking!!!!!!!

ryan-mm85 wrote:

so its printing well with ABS, but the resolution of the layers is horrible. they are rough.
any ideas why this is happening.

Pics?
This could be a number of things, many being quite simple fixes

Printit Mason and Printit Horizon printers
Multiple SD2s- Bulldog XL, E3D v5/v6/Lite6, Volcano, Hobb Goblin, Titan, .9 motor, Lawsy carriages, direct Y drive, fishing line...the list goes on
Filawinder and Filastruder #1870.....worth every penny!

33

Re: so been away awhile, first layer not sticking!!!!!!!

here is the layers in .3 they are rough not stacking well,

almost like there is a little banding. I only remember the term not what causes it,
its not z band because I have my slop nut in place

Post's attachments

DSC00005.JPG 138.67 kb, file has never been downloaded. 

DSC00006.JPG
DSC00006.JPG 131.22 kb, file has never been downloaded. 

DSC00007.JPG 139.92 kb, file has never been downloaded. 

DSC00008.JPG
DSC00008.JPG 136.06 kb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

34

Re: so been away awhile, first layer not sticking!!!!!!!

wardjr wrote:

Then set your first layer height in your slic3r profile to .2963 set other layers to that same number.  Then try a print and stop it right after it makes the first loop.

what should I set them for .1  and .2 settings?

35

Re: so been away awhile, first layer not sticking!!!!!!!

ryan-mm85 wrote:
wardjr wrote:

Then set your first layer height in your slic3r profile to .2963 set other layers to that same number.  Then try a print and stop it right after it makes the first loop.

what should I set them for .1  and .2 settings?

Use this calculator
http://prusaprinters.org/calculator/#steppers

Scroll down to optimal layer height for z axis and select 5/16-18 as the pitch preset. The z motor is 1.8 step angle so leave that at its default.

36

Re: so been away awhile, first layer not sticking!!!!!!!

jagowilson wrote:
ryan-mm85 wrote:
wardjr wrote:

Then set your first layer height in your slic3r profile to .2963 set other layers to that same number.  Then try a print and stop it right after it makes the first loop.

what should I set them for .1  and .2 settings?

Use this calculator
http://prusaprinters.org/calculator/#steppers

Scroll down to optimal layer height for z axis and select 5/16-18 as the pitch preset. The z motor is 1.8 step angle so leave that at its default.

I have no idea what any of these numbers are for an SD3

37 (edited by jagowilson 2015-02-08 18:22:52)

Re: so been away awhile, first layer not sticking!!!!!!!

All you have to do is fill it out like I described. See attached image. This is for .1mm layer height.

Post's attachments

image.jpg
image.jpg 111.56 kb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

38 (edited by ryan-mm85 2015-02-08 18:38:38)

Re: so been away awhile, first layer not sticking!!!!!!!

so I want to use the .09878 or the .1058?

39 (edited by jagowilson 2015-02-08 18:39:48)

Re: so been away awhile, first layer not sticking!!!!!!!

Doesn't matter. Id go with the larger one just because fewer layers = shorter printing time.

40

Re: so been away awhile, first layer not sticking!!!!!!!

ryan-mm85 wrote:

here is the layers in .3 they are rough not stacking well,

almost like there is a little banding. I only remember the term not what causes it,
its not z band because I have my slop nut in place

so any ideas on this question?

its from a previous post of mine.