Topic: Tweaking Tips Needed
So I've got my extruder and flow calibrated, and I think that they are almost perfect.
However, I think I am stuck on getting retraction tweaked. I've done about 40 test prints of the 40x10.stl file, and I still end up with plastic dingleberries all over my print.
As you can see in my photo, I seem to have nice, strong edges, but in other places, I have plastic loops sticking out.
I am printing at 180C and my retraction settings are:
Length: 1.25mm
Lift Z: 0
Speed: 300mm/s
Extra length on restart: 0.6mm
Min travel after retraction: 0.5mm
With all of my test prints, if I would change these settings too much, I would end up with more of a blob than the test print. These are the settings that "seemed" to do best, but not perfect.
What are the best ways to get rid of these dingleberries?
Thanks!