What's The best glue stick to use
Purple
I have a xyzprinting DUO 2.0. I have tried blue tape, UHU stic Glue Stick and nothing. This month I discovered Elmers Craft BOND Extra Strength permanent bond glue stick. It works great. I seldom clean the glass and just reapply more Elmers after removing the item and scraping the glass with a painters 6 in 1 tool, usually when still hot. Objects stick very well. They can sometimes be a little hard to remove.