Topic: Sticking issue during z calibration
I've tried 3 different brands of glue stick and none of the extruded filament is staying on the glass bed.
I've tried Elmer's washable school glue (disappearing purple), Elmer's extra strength glue stick and Scotch craft stick. I wash the bed between attempts and apply the glue when the bed is cool. I also remove the filament hanging on the nozzle. Attached is a photo of the filament just staying on the nozzle after a z calibration attempt.
Any thoughts on what I should try next?