Topic: Slic3r help
I made 2 prints today use the models from Make magazine used to test the printers. I ran one through the XYZ software and one through slic3r using similar settings. The XYZ print came out looking better. The one on the right was from slic3r. I have them both set at .2mm, 10% infill. I'm not sure what the speed differences are but XYZ was set at normal speed and slic3r was set at 40 mm/s. XYZ used the default of 220 temp for the extruder and I had slic3r set at 210.
Any help on understanding why such a difference in prints would be greatly appreciated. The print from slic3r also came out with ABS strands coming off 2 corners.
Thanks!