1

Topic: Glob of filament gattering on tip, first layer?

Hi when printing I keep getting a glob of filament collecting on the tip during the first layer?  idea why that is?

2

Re: Glob of filament gattering on tip, first layer?

hansen644 wrote:

Hi when printing I keep getting a glob of filament collecting on the tip during the first layer?  idea why that is?

It happened to me in the beginning, but went away when I did a bed calibration.  Might try that if it has not been done in a while.  Im a beginner so may be better answers out there.

DaVinci 2.0 Duo
Latest Stock Software
XYZ ABS only
1st print 12/26/14

3 (edited by carl_m1968 2015-01-12 18:21:28)

Re: Glob of filament gattering on tip, first layer?

hansen644 wrote:

Hi when printing I keep getting a glob of filament collecting on the tip during the first layer?  idea why that is?

It could be possible your bed is too close to the nozzle and a bit of filament is rolling up on to the nozzle.  The trick is there is getting close enough to get a proper stick but not so close that it is causing your problem. I use a feeler gauge to set my bed at .15 which is perfect for most of the print option the Da Vinci is capable. If you wanted to print a .1 or lower then you would need to go down to a .05 space. However I do not believe the Da Vinci is capable of .1 or less layer heights with the stock extruder and mainboard. It claims it can do it but I doubt the layers are actually .1 when measured.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

4

Re: Glob of filament gattering on tip, first layer?

yep like carl said. this only happens when the bed is too close to the nozzle .