Topic: Raftless not sticking to bed
I've tried a few different temperature combinations since I got my Solidoode 2 (with heated bed) a few weeks ago but cannot seem to get the filament to stick unless I add a raft in Skeinforge. Every time I try to print without the raft the very first drop of plastic sticks to the head of the extruder and and is drug around the bed for a split second as seen in this video:
youtu.be/2nQfsk7yOYg
In this video the first 2 runs were at:
Extruder: 185c
Bed: 100c
And the last 3 were:
Extruder: 175c
Bed: 100c
I've tried other temperatures in the past with the same results.
Even when I print with a raft the first drop lifts up off the bed but not as much (I guess since it's thicker) and since it's on the "outskirts" of the object the rest of the print job is not affected.
Any thoughts?
Thanks!