Topic: Suggestion request for nozzle size, 3-4 to drill.
So my main concern is for 3mm pla, I use the 3mm melt filter for abs and get great results on both vertical and horizontal with a slight slope. Pla comes out around 2.2mm on the same setup with 3 fans, i've drilled one for 1.9mm and get great results on vertical with winder for pla/abs coming out around 1.8mm, but might want to drill some around 1.8mm.
have 3 undrilled nozzle's i'd like to drill for pla and other materials that have a slower cooldown time.
any suggestions from experience would be great at this point before i just go drilling away.
will be using a drill press at work so i'll have to pickup the bits first and will post results once there in.
feel free to post any suggestions for all sizes you'd like to see as well.