Topic: New Nozzle = strange behaviour
So after clogging my nozzle a couple of times and finally not being able to get it cleaned out well enough, I bought a new nozzle and put everything back together again. After trying a few prints with this strange behavior, I went back through the calibration process and found that the cube I printed had a wall thickness of .35 and not .42 like I expected. So is that thinner thread what is causing the strange prints with threads not even close to each other? I tried adjusting the Extrusion Multiplier up above 1 to increase the wall thickness but it didn't do anything. Does anyone have a suggestion on what I should check.
Thanks in advance!
FYI I also have a Robo3D and the support by the company and by the forum users is terrible. I can't thank you all enough for the welcome and friendly responses I have received here!!!