1

Topic: SD4 bottom surface twisting

whenever I tried to build modes bottom surface  was twisted and make next layers fucked up. I don't know why and how to figure it out

Post's attachments

사진 1 (1).JPG
사진 1 (1).JPG 1.78 mb, file has never been downloaded. 

사진 2.JPG
사진 2.JPG 1.73 mb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

2

Re: SD4 bottom surface twisting

Please watch the profanity.

You are experiencing lifting which has been covered dozens of times here. What surface are you printing on?