Topic: just a little off....
Hey everyone, I've been messing with my Davinci 1.0 for two weeks now and am trying to figure out this "out of round" hole issue. I've tightened belts, adjusted the Y drive motor belt, shimmed the pulley, adjusted X belt, X pulley (the white one) but am still getting slightly out of round holes and my parts are a little short in the Y direction. When printing a 40 x 40mm square, I get 40.00 to 40.1 in the X, but 39.8 in the Y.
So my Y axis is around 0.2 to 0.3mm smaller than the X. Am I just an extreme perfectionist or can the DA Vinci do better? I am not sure what else to try (hardware wise) to get the print to come out closer.
On a final note, I have until Monday to take it back to the store to exchange for a new one, .3mm seems small for a bad apple but if people are having better luck maybe its worth a shot?