Topic: SD4 top layer infill issues
so i have got my new E3DV6 installed and extruding correctly. my hollow cube wall thicknesses are .42 exactly.
but i am having a couple issues.
1. my top layers are not filling 100% the tops do not meet up with the perimeters at all times. ( see picture)
2. my 10mm x 10mm test cubes are 10mm on 2 sides and 9.5mm on the other 2 sides. what is causing this?
my extruderis correctly calibrated and i have tensioned my belts evenly.