Topic: switching from ABS to PLA
Whats the biggest things i need to change to switch over to PLA besides material haha. So far never ran any PLA through my system, only ABS. Thanks for the tips.
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → Help/Repair/Maintenance → switching from ABS to PLA
Whats the biggest things i need to change to switch over to PLA besides material haha. So far never ran any PLA through my system, only ABS. Thanks for the tips.
Change your extruder temp to the filament manufacturer's recommendation. Heat your bed to about 60 C or so. Personally, I don't like printing in PLA so I avoid it whenever possible.
Personally, I don't like printing in PLA so I avoid it whenever possible.
+1
Also, PLA tends to clog more on a stock SD hot end...and you will likely need a cooling fan for the nozzle as PLA cools more slowly.
I print PLA at 220c (190c if you are still using the stock hotend) and 60c for the bed.
You will need a fan to actively cool the layers as IronMan mentioned. You could either print a fan mount, which is easy since designs are abundant on Thingiverse, or just use a desk fan if you remove your enclosure.
+1 on the clogs.
be careful using pla with the stock hotend. Azerate can attest to my issues. 2nd time i used it it clogged my head and i killed it trying to gently take it apart. plinting in pla right now with a e3d. no heat on the bead and other than the damn spool binding up and coming off the reel, its printing fine
I have the old SD2 and PLA extruder temp was set at 180-185c and bed at 60c but I too likely wont use PLA again at least on my old SD2. I like ABS finished results and durability way better for my printing needs.