1

Topic: New filament for da vinci,Prints coming out thinner, stringy, stretchy

hey guys,

I changed filament today with a cartridge resetter.... I am now using boots industries top notch filament, which is 1.75mm white abs. when I made a test print, the print came out very stringy, barely infilled, and separated from each layer, making it almost stretchy. does anyone know what settings I would have to change in slic3r to make this new filament work like the xyzprinting cartridge work, which was a lot better?

heres some pics:

First picture shows new filament on the left, xyz on right.

Thanks
Alex

Post's attachments

image.jpg
image.jpg 688.78 kb, 1 downloads since 2014-09-18 

image.jpg
image.jpg 1.14 mb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

2

Re: New filament for da vinci,Prints coming out thinner, stringy, stretchy

I'm using a resetter and had the same problem, see the topic 'filament-coming-out-blotchy' still on the front page of the forum for XYZ Printing DaVinci

I got it to work for a while, then had to disassemble my extruder head to clean it (Not sure if the need to clean was related or if it was my homemade filament)

3

Re: New filament for da vinci,Prints coming out thinner, stringy, stretchy

What temperatures are you using? So far I've had better luck running non-XYZ filament with a higher temperature than the stock cartridge calls for. I think the default is 210, Currently I'm running at 230C with the heated bed at 115 with kapton to prevent warping.

Also on a side note, check to make sure your belts are tight, and that you do not have any cracked pulleys!

4

Re: New filament for da vinci,Prints coming out thinner, stringy, stretchy

just checking here to see if this issue was ever resolved? I am having th EXACT same problem right now only i am using the hatchbox ABS filament.

My printers are almost spongy

5

Re: New filament for da vinci,Prints coming out thinner, stringy, stretchy

I have purchased three other types of filament, and they beleive its a problem wth the extruder multiplier. I'm going to try to screw with it after canadian thanksgiving.

6

Re: New filament for da vinci,Prints coming out thinner, stringy, stretchy

What version of software and firmware are you running.  This looks to me to be a non-filament based issue.  Also verify your belts have the proper tension.  My printer was missing the screw on the X-Axis that locks it into place when I got it, which was causing some issues like this only not nearly as severe.

7

Re: New filament for da vinci,Prints coming out thinner, stringy, stretchy

Looks like a typical problem with firmware J.
Revert back to firmware G should solve your problem

8

Re: New filament for da vinci,Prints coming out thinner, stringy, stretchy

Wow, ok, thanks for all the recommendations, I will revert to firmware g, and adjust the tightness.

I appreciate it guys
Alex