1 (edited by Nerfz 2014-09-22 15:17:53)

Topic: Return SD4?

So far I have had really bad luck with the Solidoodle 4 I received on Thursday.. The Y axis were put together wrong so it would not move... Z axis step tab not in the right place that was causing my bed to be lop sided...And now the tip gets clogged every 5 passes and cannot complete a print...Ahhh!!!

What should I do?

And yes I know that it would be some work to get this thing going but jeez I did not expect as many factory mistakes....

SD4, Glass bed,(Soon to have) E3D v6, MK5 extruder

2

Re: Return SD4?

Shipping can really knock things around as well.
If you clogged your hot end from leaving it on too long then you'll want to look at this post
http://www.soliforum.com/topic/255/clea … esnt-work/
As far as belt alignment for the Y-axis goes there is no good way to put it into words.  I like to tension the belts about the same on each side.  Then loosen a set screw on the rear right drive pulley.  Slide the whole gantry back and forth stopping near the middle and with that right side in a nice neutral position.  Tighten the set screw and that should solve any Y-axis skipping issues.  If the X-axis is skipping check the Teflon blocks that slide on the rear rod to make sure they aren't binding or to tight.

Printit Industries Model 8.10 fully enclosed CoreXY, Chamber heat
3-SD3's & a Workbench all fully enclosed, RH-Slic3r Win7pro, E3D V6, Volcano & Cyclops Hot End
SSR/500W AC Heated Glass Bed, Linear bearings on SS rods. Direct Drive Y-axis, BulldogXL
Thanks to all for your contributions

3

Re: Return SD4?

I fixed the belts who ever assembled it clamped it down at and angle...So I fixed Axis issues.. It works fine but after say 5 layers it clogs.. I think the tip might be bad...It will be putting down perfect lines then boom nothing...

SD4, Glass bed,(Soon to have) E3D v6, MK5 extruder

4

Re: Return SD4?

Could be moisture in your filament also.  How humid has it been in your area?
What temp are you running it at and are you using ABS or PLA?

Printit Industries Model 8.10 fully enclosed CoreXY, Chamber heat
3-SD3's & a Workbench all fully enclosed, RH-Slic3r Win7pro, E3D V6, Volcano & Cyclops Hot End
SSR/500W AC Heated Glass Bed, Linear bearings on SS rods. Direct Drive Y-axis, BulldogXL
Thanks to all for your contributions

5

Re: Return SD4?

A little humid.. Running abs at 210-215 tried 195 also same thing.. Using Solidoodle black abs...

SD4, Glass bed,(Soon to have) E3D v6, MK5 extruder

6

Re: Return SD4?

Humid here but not in the area inside where I use it...

SD4, Glass bed,(Soon to have) E3D v6, MK5 extruder

7

Re: Return SD4?

Once the filament strips it leaves plastic in the cogs of the drive gear.  You might want to start by using a brush to clean that off first.  You can put your filament in the oven for a while to dry it out for a couple of hours have a search on that to see what temps are working best for people.
Also you could be over extruding causing too much back pressure on the nozzle.  Have you done any of the calibrations for the extrusion side (steps per mm and extrusion multiplier)?

Printit Industries Model 8.10 fully enclosed CoreXY, Chamber heat
3-SD3's & a Workbench all fully enclosed, RH-Slic3r Win7pro, E3D V6, Volcano & Cyclops Hot End
SSR/500W AC Heated Glass Bed, Linear bearings on SS rods. Direct Drive Y-axis, BulldogXL
Thanks to all for your contributions

8

Re: Return SD4?

No I have not calibrated that...Hmmm I guess it could be that.... Mind posting a link for it?

And thanks you...

SD4, Glass bed,(Soon to have) E3D v6, MK5 extruder

9

Re: Return SD4?

Just look in the WIKI but here are the links
https://www.youtube.com/watch?v=JZGdMc2ebPo
http://www.soliwiki.com/Calibration_of_the_flow_rate

Printit Industries Model 8.10 fully enclosed CoreXY, Chamber heat
3-SD3's & a Workbench all fully enclosed, RH-Slic3r Win7pro, E3D V6, Volcano & Cyclops Hot End
SSR/500W AC Heated Glass Bed, Linear bearings on SS rods. Direct Drive Y-axis, BulldogXL
Thanks to all for your contributions

10

Re: Return SD4?

Thanks a lot we will see if that works...

SD4, Glass bed,(Soon to have) E3D v6, MK5 extruder

11 (edited by Nerfz 2014-09-23 01:12:17)

Re: Return SD4?

So I took apart the exstruder and the whole inside is melted to the peek insulator piece? So looks like the exstuder is dead!
And a new one is $59.00 and they are out of stock wtf...

SD4, Glass bed,(Soon to have) E3D v6, MK5 extruder

12

Re: Return SD4?

Nerfz wrote:

So I took apart the exstruder and the whole inside is melted to the peek insulator piece? So looks like the exstuder is dead!
And a new one is $59.00 and they are out of stock wtf...

Photos?

13

Re: Return SD4?

I can e-mail you pics if you want.. Don't see an upload button on here... But I popped the barrel and nozzle off the peek insulator and the insulator was melted on the inside.. I can't push filament through it....

SD4, Glass bed,(Soon to have) E3D v6, MK5 extruder

14

Re: Return SD4?

Nerfz wrote:

So far I have had really bad luck with the Solidoodle 4 I received on Thursday.. The Y axis were put together wrong so it would not move... Z axis step tab not in the right place that was causing my bed to be lop sided...And now the tip gets clogged every 5 passes and cannot complete a print...Ahhh!!!

What should I do?

And yes I know that it would be some work to get this thing going but jeez I did not expect as many factory mistakes....

Let's be serious!

You just payed on the close order of $700 for a piece of worthless junk that failed right out of the box!

What in the wildest realm of imagination would cause you any doubt about what you should do?!

Let's put the question in perspective. What would you do with a $10 toaster you bought at Walmart if it was defective out of the box? What would you do with a $700 kitchen appliance, stereo or TV that was factory defective junk before you even unpacked it and plugged it in?

I don't get it. I really don't. Why would anyone tolerate anything less than a fully functional, properly working product with any brand new merchandise costing that much money?!

15

Re: Return SD4?

When still using my PEEK, I straightened out a section of a coat hanger, heated it up, then plunged it through the clogged area. But stock SD hotend has its flaws.
If you upgrade to an E3D, found Here , it costs $79, is currently in stock, allows you to print more materials than the stock would allow, and is difficult to clog. You seriously have to try to clog the sucker. Since then, I never used a coat hanger.

But if you JUST got your SD4, I recommend clearing the clog then properly calibrating everything. It sucks to be impatient with your new machine, but the results will be night and day. The links wardjr gave should be enough to get you printing properly once said clog is a memory.

Printit Mason and Printit Horizon printers
Multiple SD2s- Bulldog XL, E3D v5/v6/Lite6, Volcano, Hobb Goblin, Titan, .9 motor, Lawsy carriages, direct Y drive, fishing line...the list goes on
Filawinder and Filastruder #1870.....worth every penny!

16

Re: Return SD4?

The Peek insulator(The guide for the filament melted to the nozzle..I think it's toast.. I am going to talk to support again tomorrow... I mean I really want the printer.. seems better then others I would get for that price...(As long as I can get it going..

SD4, Glass bed,(Soon to have) E3D v6, MK5 extruder

17

Re: Return SD4?

Nerfz wrote:

I can e-mail you pics if you want.. Don't see an upload button on here... But I popped the barrel and nozzle off the peek insulator and the insulator was melted on the inside.. I can't push filament through it....

www.imgur.com

18

Re: Return SD4?

elmoret wrote:
Nerfz wrote:

I can e-mail you pics if you want.. Don't see an upload button on here... But I popped the barrel and nozzle off the peek insulator and the insulator was melted on the inside.. I can't push filament through it....

www.imgur.com

+1
Start an account at the site elmoret gave.
Upload an image to your account. When you select your desired image, there will be a series of codes on the right hand column. Copy the code for "forums" and paste it into the massage box here to insert it into your message.

Printit Mason and Printit Horizon printers
Multiple SD2s- Bulldog XL, E3D v5/v6/Lite6, Volcano, Hobb Goblin, Titan, .9 motor, Lawsy carriages, direct Y drive, fishing line...the list goes on
Filawinder and Filastruder #1870.....worth every penny!

19

Re: Return SD4?

Ask yourself what you really want out of your printer.  Then upgrade to an E3d as there are plenty of users here to help.  Do some research and read the WIKI section on the E3d.  It is definitely a project but well worth the effort.  In the long run you will want this upgrade and I'm sure SD will take care of you but your time maybe better spent just taking matters into your own hands. 
As far as comments about toasters and other appliances purchased at Walmart go,  I wonder when the first commercially available toaster became available to the general public?  And the first printers sold to the masses started when? Hardly seems like a fair comparison.
This is rapidly evolving technology but it is a complex machine and requires a certain skill set to be able to operate successfully.  I wouldn't expect to walk into the local machine shop and be able to run their CNC successfully because I'm not a machinist.  In fact I'm sure I would walk away thinking their machine was junk because I couldn't make it work or I'd come to the realization that maybe I didn't know what I was doing.  At that point I could take two different paths.
1. I could learn how to operate the machine.
2. I could become bitter and take every opportunity to bad mouth the machine and the company that manufactured it.
Could SD do things better?  You bet. 
Are they trying to improve?  The last year has proven they are.  Many of the mods that came directly from this forum are showing up on the new models.
To get back to the OP
It sounds like you want to make your printer not only work but work well, how can I help make that happen?

Printit Industries Model 8.10 fully enclosed CoreXY, Chamber heat
3-SD3's & a Workbench all fully enclosed, RH-Slic3r Win7pro, E3D V6, Volcano & Cyclops Hot End
SSR/500W AC Heated Glass Bed, Linear bearings on SS rods. Direct Drive Y-axis, BulldogXL
Thanks to all for your contributions

20

Re: Return SD4?

Where is the like Button??????lol
Yes you are correct..And that is why I did not comment on his post...Even a lot of kits from china cost $700 without a good foundation And I also realize all of this is new even to the company making it...
I do not mind upgrading because I definitely want to be able to print on a lot of different filaments..


Thanks a lot guys this is a great community!

SD4, Glass bed,(Soon to have) E3D v6, MK5 extruder

21 (edited by Nerfz 2014-09-23 20:31:25)

Re: Return SD4?

Can't see in the insulator but if you look at the right hand side of the nozzle you will see the melted white plastic... The the entire inside of the insulator is shot..

Post's attachments

20140922_213414.jpg
20140922_213414.jpg 2.44 mb, file has never been downloaded. 

20140922_213533.jpg
20140922_213533.jpg 2.23 mb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.
SD4, Glass bed,(Soon to have) E3D v6, MK5 extruder

22

Re: Return SD4?

Have to give some Prop's to Solidoodle they are sending me out new parts and standing behind their product!

SD4, Glass bed,(Soon to have) E3D v6, MK5 extruder