Topic: weird artifacts
Here's an STL Im trying to print: http://www.solidoodles.com/uploads/doodle?id=424
Can someone explain what these strange artifacts are and how to prevent them?:
highlighted in red
close up:
solidoodle ABS, 0.3mm layer height, Repetier Host, sliced with Slic3r.
This artifact was even more noticeable when I printed a Z axis adjuster replacement. http://www.thingiverse.com/thing:281477
The two holes where the screws had to go had similar holes on their sides, they were even see-through at places.