1 (edited by perlguy 2012-12-08 19:12:30)

Topic: First .1mm attempt, need some tips

I think that I have everything calibrated and I've done all of the steps in the instructions for setting up Repetier, and then re-split my .stl file with the .1mm settings.

The print starts out looking like it is going to be awesome, but after printing a few layers, it starts looking awful and has all sorts of lines that are not sticking to the layers.

I am attaching some photos so you can see what I mean - it is easier to look at the photos than try to fully explain it all.

Based on the photos, what do you think is the problem here?  I am not sure what to check next.

Thanks!

Perlguy.

Post's attachments

IMG_0001.jpg 177.07 kb, 2 downloads since 2012-12-08 

IMG_0002_2.jpg
IMG_0002_2.jpg 142.48 kb, 2 downloads since 2012-12-08 

IMG_0003_2.jpg 130.06 kb, 3 downloads since 2012-12-08 

IMG_0004_2.jpg 128.6 kb, 2 downloads since 2012-12-08 

IMG_0005_2.jpg
IMG_0005_2.jpg 145.48 kb, 2 downloads since 2012-12-08 

You don't have the permssions to download the attachments of this post.

2

Re: First .1mm attempt, need some tips

does the .3mm profile work correctly?

3

Re: First .1mm attempt, need some tips

Yes, .3mm seems to work just fine.

4

Re: First .1mm attempt, need some tips

Try slowing it down, plastic may be staying to hot as layer goes on top of layer, eventually getting those mushy edges you see.

5

Re: First .1mm attempt, need some tips

I tried slowing it down by changing the Speed settings in Slicer (under Print Settings).

I then tried it on 2 different prints, just in case the first one that I had was messed up somehow.

On both prints, the first few layers (3 or 4?) seem to go down perfect - then all hell breaks loose.  The edges then start to look more like "lava rock", than anything else.

Am I missing something?  Doing something wrong?  I am still VERY new to this whole process and really want to learn!

I am again putting photos in this post so that you can see what I mean.

Thank you!
Perlguy

Post's attachments

photo 1.JPG
photo 1.JPG 141.52 kb, 2 downloads since 2012-12-09 

photo 2.JPG
photo 2.JPG 188.14 kb, 2 downloads since 2012-12-09 

photo 3.JPG 164.09 kb, 2 downloads since 2012-12-09 

photo 4.JPG
photo 4.JPG 109.38 kb, 3 downloads since 2012-12-09 

photo 5.JPG
photo 5.JPG 334.11 kb, 3 downloads since 2012-12-09 

You don't have the permssions to download the attachments of this post.

6

Re: First .1mm attempt, need some tips

Can you post your .1mm settings?

SD2 with E3D, SD Press, Form 1+