1

Topic: sd4 problems

was printing a job it stopped during run all of a sudden.   Now the only thing it will do is go to home when push home all.   The extruder will not feed, the xyx buttons wont work only when hit home.   Start a print bed moves down then up and nothing Rephost shows it progress on screen but nothing. Thanks in advance for any help.

2

Re: sd4 problems

also uninstalled and reinstalled rephost and serial number

3

Re: sd4 problems

recheck all slicer settings that have been changed recently for mistakes doing G-code

Solidoodle 2 with Deluxe kit cover & glass bed with heater. and 2nd board SD2 used not 3rd and alum platform not installed yet still wood. also need cooling fan installed to board. use Repetier Host couple vers. Slic3r also have all free ware STL programs

4

Re: sd4 problems

checked everything got it up and running,   Printed a part was nice print then got sloppy print that u could pull apart with hand.   Temps are fluctuating bed and extruder show they get to set temp then fall.  Posting pics of screen shot and print

Post's attachments

IMG_3152.JPG 2.12 mb, file has never been downloaded. 

IMG_3153.JPG 3.95 mb, file has never been downloaded. 

IMG_3154.JPG
IMG_3154.JPG 2.58 mb, file has never been downloaded. 

IMG_3155.JPG
IMG_3155.JPG 1.79 mb, file has never been downloaded. 

IMG_3156.JPG
IMG_3156.JPG 3.97 mb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

5

Re: sd4 problems

Here is the good print.  Let me add I printed after the green mess and it went decent but print pulled apart and stopped before it finished
Thanks for any and all hellp

Post's attachments

IMG_3159.JPG
IMG_3159.JPG 1.88 mb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

6

Re: sd4 problems

I think you can try that, set extruder temp from 210-215, don't set it as 225,
Solidoodle set 230 as max. Temp, then it reached that, your printer will stop,
If we consider temp errors, it is very easy to over 230, let bed temp to be
105, try again!

7

Re: sd4 problems

Thanks