Topic: Filament Diameter (too large)
Greetings all
So i've extruded a few Kg's (2-3) of filament already, but now that im printing with it, i seem to be having problems.
The initial filament i didn't use as its recommended to clean out the system, and thereafter the filament worked in my printer, this must have been approx 300-500g of filament. However everything that i have made after that doesn't work in my printer, it gets stuck at the extruder due to its size.
Filament that i have purchased, ABS and PLA 1.75mm works fine. Printer nozzle is 0.4mm.
Any ideas suggestions thoughts would be much appreciated.
Thanks in advance.