Printed this skull at .1 (with support, that has been removed), and I'm getting some assymetrical distortion. It was printed from the rear of the skull up. Notice the way the head appears to be "squished" and what's really interesting is how one side is almost perfect, but the other has vertical banding. The eyes are different shapes.
Any suggestions?
Post's attachmentsphoto 1.JPG 373.78 kb, file has never been downloaded.
photo 2.JPG
photo 2.JPG 301.43 kb, file has never been downloaded.
photo 3.JPG
photo 3.JPG 257.07 kb, file has never been downloaded.
photo 4.JPG 280.17 kb, file has never been downloaded.
Screen Shot 2014-08-26 at 7.48.46 AM.png
Screen Shot 2014-08-26 at 7.48.46 AM.png 78.34 kb, file has never been downloaded.
You don't have the permssions to download the attachments of this post.
Stock SD4 with 3/16" glass attached to stock (kapton-covered) bed with Aquanet.